1、使用冷再生機施工前要調好水泥漿的稠度并拌合均勻,水泥漿中的雜質和硬塊應用濾網濾出,以免堵塞噴嘴;事先調試好噴嘴的噴漿量,以保證水泥劑量準確。
1. Before using the cold regenerator for construction, the consistency of the cement slurry shall be adjusted and mixed evenly. The impurities and hard blocks in the cement slurry shall be filtered out through the filter screen to avoid blocking the nozzle; Adjust the spraying quantity of the nozzle in advance to ensure the accurate cement dosage.
2、開始施工時速度不要太快,為滿足設計和質量要求,要經常檢查拌合的均勻情況和深度,發現與設計有差異時要及時調整。
2. Do not start construction too fast. In order to meet the design and quality requirements, the uniformity and depth of mixing shall be checked frequently, and timely adjustment shall be made in case of any difference from the design.
3、作業施工水罐車停車時一定要離開已施工或待施工水泥已攤鋪路面,以防止漏水引起的局部水大。
3. When the construction water tanker stops, it must leave the paved road of cement that has been constructed or to be constructed, so as to prevent large local water caused by water leakage.


4、施工車輛停放時一定要錯開第二天的段道預工作面,以防止耽誤第二天的人工水泥攤鋪。
4. When parking construction vehicles, the first pre working face of the first section of the next day must be staggered to prevent delaying the artificial cement paving of the next day.
5、避免犯"過壓"的錯誤,即過度壓實。若達到材料的大密實度后仍然繼續碾壓,則會破壞材料,反而降低其密實度。
5. Avoid the mistake of "overpressure", i.e. over compaction. If the rolling is continued after reaching the maximum compactness of the material, the material will be damaged and its compactness will be reduced.
6、冷再生機的施工作業應該在每天下午15:00-16:00之間結束,以便后續施工能在天黑前結束。
6. The construction of cold regenerator shall be completed between 15:00 and 16:00 every afternoon, so that the subsequent construction can be completed before dark.
7、每天冷再生機結束施工進行洗刀停車后,應通知操作手仔細檢查車況并更換刀頭,以免耽誤第二天的施工進度。
7. After the construction of the cold regenerator is finished and the tool is washed and stopped every day, the operator shall be notified to carefully check the vehicle condition and replace the tool head, so as not to delay the construction progress of the next day.
8、冷再生機拌合過程中要經常檢查拌合機刀頭的磨損情況和水泥漿車的噴嘴,刀頭磨損嚴重要及時更換,噴嘴發生堵塞要及時疏通。
8. During the mixing process of the cold regenerator, the wear of the cutter head of the mixer and the nozzle of the cement slurry truck shall be frequently checked. If the cutter head is seriously worn, it shall be replaced in time, and the nozzle blockage shall be dredged in time.
9、冷再生機拌合時將整個半幅分成3次拌合,用完水泥漿車內已知重量水泥后,核算已經作業的面積與水泥消耗是否相符,及時做出調整。作業結束,放出剩余水泥漿。
9. When mixing with the cold regenerator, divide the whole half into three times. After using up the known weight of cement in the cement slurry truck, check whether the operated area is consistent with the cement consumption, and make adjustment in time. After the operation, release the remaining cement slurry.
以上就是今天小編給大家提供的精彩內容,更多的精彩內容請點擊進入我們的網站:冷再生機租賃http://www.mshjwlk.com
The above is the wonderful content provided by Xiaobian today. For more wonderful content, please click to enter our official website: cold regenerator rental http://www.mshjwlk.com
下一篇:路面冷再生機的組成介紹 上一篇:泡沫瀝青發泡監理要注意什么?
閱讀/ Recommended reading
- 冷再生機租賃故障應對:全流程解決指南 2025-07-04
- 水泥撒布車料倉:讓存量監測成為 “一目了然的智慧管家” 2025-07-03